After applying the carbon mats a thermal process is carried out. At a pressure of 5 bars and a temperature of 125 °C the wheel is allowed to set for 4 hours and it is within this process that the wheel gets it unmistakeable shinning Carbon look.

TEST_Herstellung_03

When the wheel is set it is then mechanically worked to set the tyre seating and checked for total quality.